Warning: Undefined array key "HTTP_ACCEPT_ENCODING" in /mnt/web508/d3/15/536615/htdocs/relaunch.mbe-komponenten.de/includes/general.inc.php on line 15 Deprecated: preg_match(): Passing null to parameter #2 ($subject) of type string is deprecated in /mnt/web508/d3/15/536615/htdocs/relaunch.mbe-komponenten.de/includes/general.inc.php on line 15 Migration enhanced MBE - Glossary - Dr. Eberl MBE-Komponenten GmbH
Glossary
Glossary
MBE process but, with alternate deposition of the constituent elements (i.e. with monolayer by monolayer growth interruptions). The interruped deposition allows surface migration, which results in planarization during epitaxial growth.